The domestic machine washing will make the Lyocell fabric increase in thickness and area weight but decrease in density.
家用洗涤将使织物的厚度、平方米重增大,体积重量减小;
When the coagulation bath concentration is 10%, the maximum of tenacity and modulus and the minimum of extension at break of Lyocell fiber are obtained.
而在凝固浴浓度为10%时,纤维的相对强度和初始模量为最大,延伸度则为最小。
This moderate and low MW cellulose acted as the plasticiser, which made the process easier, and the high MW section endued Lyocell fibers with good mechanical properties.
这些中低相对分子质量部分的纤维素起了增塑作用,使加工更容易,而高相对分子质量部分则赋予纤维良好的力学性能。
Based on the factor analysis of six characteristic parameters used to identify cotton and ramie fibers, two indirect characteristic parameters of cotton and Lyocell fibers are extracted.
本课题主要研究系统在纤维识别种类上的扩展,对系统用于识别苎麻和棉的六个特征参数进行因子分析,提取出两个有效的间接特征参数。